Scandium

Scandium Oxide

CAS #: 12060-08-1

Molecular Formula: Sc2O3

EC No.: 235-042-0

                
Contact us
Service Hotline+86-400-6632276

Product Details

Scandium oxide, chemical formula Sc2O3, pure product is white, impure product is slightly yellow powder, insoluble in water and alkali, soluble in acid. Micro hygroscopicity, easy to absorb water and carbon dioxide from the air, becoming basic scandium carbonate.

Applications:

1. Additives used in alloy materials. Aluminum scandium alloy, scandium magnesium alloy, etc.

2. Additives for special scintillation crystal growth (TSAG/GGSG)

3. Used for special scintillation ceramics.

4. Activator used in new light source materials.

5. Additive for scandium stabilized zirconium.


Product Series

ProductProduct CodeSecurity DataTechnical Data
Scandium Oxide 99.9%ET-Sc-01

Scandium Oxide.pdf

Scandium Oxide Sc2O3 99.9%.pdf

Scandium Oxide 99.99%ET-Sc-02

Scandium Oxide Sc2O3 99.99%.pdf

Scandium Oxide 99.999%ET-Sc-03

Scandium Oxide Sc2O3 99.999%.pdf

Properties (Theoretical)


Molecular FormulaO3Sc2
Molecular Weight137.91
AppearanceWhite
Melting Point2,485° C (4,505° F)
Boiling PointN/A
Density3860kg/m-3
Precise Quality137.897  g/mol
Single Isotope Mass137.896564 Da


Health & Safety Information

Signal WordN/A
Risk StatementN/A
Dangerous CodeN/A
Preventive InstructionsN/A
Flash PointNNot applicable 
Risk CodeN/A
Safety StatementN/A
RTECS NumberN/A
Transportation InformationNONH
WGK Germany3


Packaging Specifications:

Standard packaging: 50 kg/drum, 500 kg/pallet, ton bags

Sample packaging: 500 g/bag, 1 kg/bottle



Scandium Oxide
About Lanthanum Metal

The production method of Scandium Oxide is mainly oxalic acid precipitation method, that is, taking Scandium chloride or Scandium nitrate solution as raw material, adjusting the Ph value to 2 with oxalic acid, adding ammonia to precipitate scandium oxalate, heating, maturing, separating, washing, drying at 110 ℃, and burning at 900~1000 ℃ to form Scandium Oxide.