Terbium  Metal

Terbium Metal

CAS #:  7440-27-9

Linear Formula: Sc

EC No.: 231-137-6

Terbium, a silver white metal with ductility, has a melting point of 1356 ° C, a boiling point of 3230 ° C, and a density of 8.22g/m3. Terbium has magnetism at room temperature. There is only one Stable nuclide in nature, and another 20 radioactive isotopes, hexagonal lattice, soluble in dilute acid, react slowly with water. Has high reactivity. It should be stored in a container or vacuum container filled with inert gas.

Application Area:

1. Industrial technology of magnetic refrigeration.

2. Magneto optical storage materials.

3. High performance neodymium iron boron additive.

Product Series

PRODUCT

Product Code

SAFETY DATA

TECHNICAL DATA

Terbium  Metal  99.9%

ET-TBM-01


Terbium Metal 99.9%

Terbium  Metal 99.99%

ET-TBM-02

Terbium Metal 99.99%

Properties (Theoretical)

Molecular Weight 158.93
Appearance Silvery
Melting Point 1356 °C
Boiling Point 3230 °C
Density 8219 kg/m ³
Solubility in H2O N/A
Electrical Resistivity N/A
Electronegativity 1.2 Paulings
Heat of Fusion 3.90 Cal/gm mole
Heat of Vaporization 70 K-Cal/gm atom at 3123 °C
Poisson's Ratio ( form) 0.261
Specific Heat 0.0437 Cal/g/K @ 25 °C
Tensile Strength 60 MPa
Thermal Conductivity 0.111 W/cm/K @ 298.2 K
Thermal Expansion (r.t.) (poly) 10.3 µm/(m·K)
Vickers Hardness 863 MPa
Young's Modulus ( form) 55.7 GPa

Health & Safety Information

Signal Word Danger
Hazard Statements H228
Hazard Codes N/A
Risk Codes N/A
Safety Statements N/A
RTECS Number N/A
Transport Information N/A
WGK Germany 3

Packaging Specifications

Finished packaging: 50 kg / barrel, 500 kg / tray

Sample packaging: 500 g / bag, 1 kg / bottle


About Terbium Metal
About Terbium  Metal

After separating terbium from other rare earth elements through ion exchange or solvent extraction technology, metallic terbium can be prepared by metal thermal reduction method. The lithium thermal reduction of rare earth chlorides is different from the Calciothermic reaction of rare earth chlorides. The reduction process of the former is carried out in the gas phase. The lithium thermal reduction reactor is divided into two heating zones, and the reduction and distillation processes are carried out in the same equipment. Anhydrous Terbium(III) chloride is placed in the upper titanium reactor crucible (also known as TbCl3 Still room), the reducing agent lithium is placed in the lower crucible, and then the stainless steel reaction tank is vacuumized to 7Pa before heating. When the temperature reaches 1000 ℃, maintain it for a certain period of time to allow TbCl3 vapor to fully react with lithium vapor, and the reduced metal terbium solid particles fall into the lower crucible. After the reduction reaction is completed, only heat the lower crucible and distill LiCl into the upper crucible. The reduction reaction process usually takes about 10 hours. In order to obtain purer metal terbium, the reducing agent metal lithium needs to use 99.97% high-purity lithium and anhydrous TbCl3 from secondary distillation.

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
  • Subject :

Send
Related Products
Terbium Oxide

CAS #: 12037-01-3

Linear Formula: Tb4O7

EC No.: 234-856-3

Terbium Fluoride

CAS #: 13708-63-9

Linear Formula: TbF3

EC No.: 237-247-0

Terbium Chloride

CAS #: 13798-24-8

Linear Formula: TbCl3• 6H2O

EC No.:233-132-4